Gabatarwa zuwa ragar waya mai walda

Gabatarwa ga galvanized waldadin ragar waya

1. Abu: high quality waya (low carbon karfe waya).

2. Tsari: Ana yin ta ta ainihin fasahar injina mai sarrafa kansa.

3. Features: The galvanized welded waya raga yana da kyau lalata juriya da kuma yana da abũbuwan amfãni cewa general waya raga ba shi da.

4. Amfani: Ana iya amfani da shi a cikin cages na kaji, kwanduna kwai, shingen tashar, magudanar ruwa, shingen shinge, raga-hujja na bera, murfin kariya na inji, dabbobi da tsire-tsire masu tsire-tsire, grids, da dai sauransu, ana amfani da su sosai a masana'antu, noma. gine-gine, sufuri, ma'adinai da sauran masana'antu.

5. Rarraba: Dangane da matakai daban-daban na galvanizing, ana iya raba shi zuwa:

(1) Cold-galvanized welded wire mesh: Har ila yau, ya hada da sanyi-galvanized waldan waya raga da kuma bayan sanyi galvanized welded waya raga.1Farkon sanyi-galvanized welded waya raga ana waldasu kai tsaye cikin gidan yanar gizo tare da waya mai sanyi.Ba ya buƙatar jiyya na saman ƙasa da marufi don zama ragar waya mai waldadi.2 Bayan sanyi-galvanized welded waya raga da aka welded da low-carbon karfe waya sa'an nan kuma wuce ta hanyar sunadarai.Kunshin galvanized na dauki ya zama ragar waya mai waldadi.

(2) Zafi-tsoma galvanized galvanized walda waya raga: Har ila yau, ya hada da zafi-tsoma galvanized galvanized walda waya raga da post-galvanized welded waya raga.Tsarin galvanizing mai zafi da waldawa iri ɗaya ne da na sama.

Babban bambance-bambance da hanyar nuna wariya tsakanin raƙuman wariyar walda mai zafi-tsoma galvanized da ragamar walda mai sanyi-galvanized.

Babban bambanci

Hot-dip galvanizing shine a narkar da zinc a cikin yanayin ruwa, sannan a nutsar da substrate ɗin da za a yi plated, ta yadda zinc ɗin ya zama Layer interpenetrating tare da substrate don a yi masa plated, ta yadda haɗin ke da ƙarfi sosai, kuma babu ƙazanta ko ƙazanta. lahani ya kasance a tsakiyar Layer, kuma kauri na rufi yana da girma, zai iya kaiwa 100μm, don haka juriya na lalata yana da girma, gwajin gishiri na gishiri zai iya kaiwa 96 hours, wanda yayi daidai da shekaru 10 a cikin yanayin al'ada;yayin da ake gudanar da galvanizing sanyi a yanayin zafi na al'ada, ko da yake ana iya sarrafa kauri daga cikin rufin, amma dangi Dangane da ƙarfin plating da kauri, juriya na lalata ba shi da kyau.Babban bambance-bambancen da ke tsakanin nau'ikan ragar wayoyi biyu na walda sune kamar haka:

(1) Daga saman, ragamar igiyar igiyar igiyar igiyar ruwa mai zafi mai zafi ba ta da haske da zagaye kamar ragamar welded mai sanyi-galvanized.

(2) Daga adadin zinc, ragar waya mai welded mai zafi-tsoma tana da abun ciki mafi girma na zinc fiye da na'urar walda mai sanyi-galvanized.

(3) Daga mahangar rayuwar sabis, ragamar wayan da aka yi wa welded mai zafi-tsoma tana da tsawon rayuwar sabis fiye da ragamar walda ta lantarki.

2. Hanyar ganewa

(1) Kalli da idanu: Filayen welded ɗin waya mai zafi mai zafi ba shi da santsi, kuma akwai ƙaramin shingen zinc.Filayen ramin waldar waya mai sanyi-galvanized yana da santsi kuma mai haske, kuma babu ƙaramin shingen zinc.

(2) Gwajin Jiki: Adadin zinc akan waya mai waldawar wutar lantarki mai zafi shine> 100g/m2, kuma adadin zinc akan waya waldawar wutar lantarki mai sanyi shine 10g/m2.